Compare materials

Property Aluminium 7075-T6
Density (lb/ft³) 175.4
Elastic modulus E (ksi) 10,400
Poisson's ratio ν 0.33
Yield strength (0.2 % offset) (ksi) 72.95
Tensile strength (ksi) 82.96
Elongation at break (%) 11
Thermal conductivity (BTU/h·ft·°F) 75.11
Thermal expansion coefficient (µin/in·°F) 13.11
Specific heat (BTU/lb·°F) 0.2293
Melting range (°F) 891–1,175
Hardness 150 HB
Specific strength (kN·m/kg) 179

Typical values for the stated condition. Design with specified minimum or certified values.