Compare materials
| Property | Nylon 6/6 (PA66) |
|---|---|
| Density (lb/ft³) | 71.17 |
| Elastic modulus E (ksi) | 420.6 |
| Poisson's ratio ν | 0.39 |
| Tensile strength (ksi) | 12.04 |
| Elongation at break (%) | 60 |
| Thermal conductivity (BTU/h·ft·°F) | 0.1444 |
| Thermal expansion coefficient (µin/in·°F) | 44.44 |
| Specific heat (BTU/lb·°F) | 0.3989 |
| Melting range (°F) | 491–509 |
| Specific strength (kN·m/kg) | 72.81 |
Typical values for the stated condition. Design with specified minimum or certified values.