Aluminium 6061-T6

T6 (solution treated, artificially aged) · ASTM B209 / B221

Density
2,700 kg/m³
Elastic modulus E
68.9 GPa
Poisson's ratio ν
0.33
Yield strength (0.2 % offset)
276 MPa
Tensile strength
310 MPa
Compressive strength
—
Elongation at break
12 %
Thermal conductivity
167 W/m·K
Thermal expansion coefficient
23.6 µm/m·K
Specific heat
896 J/kg·K
Melting range
582–652 °C
Hardness
95 HB
Specific strength
102.2 kN·m/kg