Brass C36000
Annealed (free-cutting brass) · ASTM B16
Properties
- Density
- 530.6 lb/ft³
- Elastic modulus E
- 14,070 ksi
- Poisson's ratio ν
- 0.31
- Yield strength (0.2 % offset)
- 17.98 ksi
- Tensile strength
- 49.02 ksi
- Compressive strength
- —
- Elongation at break
- 53 %
- Thermal conductivity
- 66.45 BTU/h·ft·°F
- Thermal expansion coefficient
- 11.39 µin/in·°F
- Specific heat
- 0.09076 BTU/lb·°F
- Melting range
- 1,625–1,652 °F
- Hardness
- —
- Specific strength
- 14.59 kN·m/kg
Typical values for the stated condition. Design with specified minimum or certified values.