AISI 4140

Annealed · ASTM A29 / A322

Density
490.1 lb/ft³
Elastic modulus E
29,730 ksi
Poisson's ratio ν
0.29
Yield strength (0.2 % offset)
60.48 ksi
Tensile strength
95 ksi
Compressive strength
—
Elongation at break
25.7 %
Thermal conductivity
24.61 BTU/h·ft·°F
Thermal expansion coefficient
6.778 µin/in·°F
Specific heat
0.113 BTU/lb·°F
Melting range
2,579–2,732 °F
Hardness
197 HB
Specific strength
53.12 kN·m/kg

Quenched and tempered 4140 reaches yield strengths of 650–1600 MPa depending on tempering.