Ti-6Al-4V (Grade 5)

Annealed · ASTM B265 / B348

Density
4,430 kg/m³
Elastic modulus E
113.8 GPa
Poisson's ratio ν
0.342
Yield strength (0.2 % offset)
880 MPa
Tensile strength
950 MPa
Compressive strength
—
Elongation at break
14 %
Thermal conductivity
6.7 W/m·K
Thermal expansion coefficient
8.6 µm/m·K
Specific heat
526 J/kg·K
Melting range
1,604–1,660 °C
Hardness
334 HB
Specific strength
198.6 kN·m/kg

Typical values for the stated condition. Design with specified minimum or certified values.