EN S355JR

Hot rolled structural steel, t ≤ 16 mm · EN 10025-2

Density
490.1 lb/ft³
Elastic modulus E
30,460 ksi
Poisson's ratio ν
0.3
Yield strength (0.2 % offset)
51.49 ksi
Tensile strength
68.17 ksi
Compressive strength
—
Elongation at break
22 %
Thermal conductivity
28.89 BTU/h·ft·°F
Thermal expansion coefficient
6.667 µin/in·°F
Specific heat
0.1099 BTU/lb·°F
Melting range
2,597–2,750 °F
Hardness
—
Specific strength
45.22 kN·m/kg

Yield and tensile strength are specified minimums; tensile strength ranges 470–630 MPa.