EN S355JR
Hot rolled structural steel, t ≤ 16 mm · EN 10025-2
Properties
- Density
- 490.1 lb/ft³
- Elastic modulus E
- 30,460 ksi
- Poisson's ratio ν
- 0.3
- Yield strength (0.2 % offset)
- 51.49 ksi
- Tensile strength
- 68.17 ksi
- Compressive strength
- —
- Elongation at break
- 22 %
- Thermal conductivity
- 28.89 BTU/h·ft·°F
- Thermal expansion coefficient
- 6.667 µin/in·°F
- Specific heat
- 0.1099 BTU/lb·°F
- Melting range
- 2,597–2,750 °F
- Hardness
- —
- Specific strength
- 45.22 kN·m/kg
Yield and tensile strength are specified minimums; tensile strength ranges 470–630 MPa.
Typical values for the stated condition. Design with specified minimum or certified values.