EN S355JR
Hot rolled structural steel, t ≤ 16 mm · EN 10025-2
Properties
- Density
- 7,850 kg/m³
- Elastic modulus E
- 210 GPa
- Poisson's ratio ν
- 0.3
- Yield strength (0.2 % offset)
- 355 MPa
- Tensile strength
- 470 MPa
- Compressive strength
- —
- Elongation at break
- 22 %
- Thermal conductivity
- 50 W/m·K
- Thermal expansion coefficient
- 12 µm/m·K
- Specific heat
- 460 J/kg·K
- Melting range
- 1,425–1,510 °C
- Hardness
- —
- Specific strength
- 45.22 kN·m/kg
Yield and tensile strength are specified minimums; tensile strength ranges 470–630 MPa.
Typical values for the stated condition. Design with specified minimum or certified values.